NBR 2860 is a copolymer of butadiene and acrylonitrile to be manufactured by cold emulsion polymerization technology of Goodyear and LG Chem. NBR 2860 is a non staining, medium Mooney, and medium low acrylonitrile polymer designed to aid in processing operations such as extrusion and press molding. And also, this grade offers excellent flexibility and elasticity in low temperature by the minimized block structure and low acrylonitrile content on polymer chain. NBR 2860 is recommended for use in industrial and automotive parts such as packing, gasket and oil hose.Information provided by LG Chemical |