MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Go Yen Chemical GY-PA-530 PVC Processing Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GY-PA-530 is a processing additive with high molecular weight acrylic copolymers which is widely applied to various PVC products such as: PVC foam, WPC products, extrusion and WPC composite materials. It can reduce foaming density, maintain the consistency of bubble structure, effectively improve the quality of porous products and increase product added value.

Features:

  • Wide processing applications
  • Excellent processing additives for plastics
  • High melting elasticity
  • High strength
  • Reduces foaming density
  • Maintains the consistency of bubble structure
  • Effectively improves quality of porous products
Applications:
  • PVC foam core tube
  • PVC foam materials
  • PVC foam reinforced composite materials
  • WPC composite materials
  • WPC related products
  • Extrusion applications

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • Density
  • Volatiles
  • Particle Mesh Size, <2%
  • Viscosity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.