MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Unifrax Isofrax® 1260C Blanket Thermal Insulation
Categories: Ceramic; Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Isofrax® Thermal Insulation from Unifrax is a fiber that utilizes a unique, patented silica-magnesia chemistry to solve a variety of demanding, high-temperature application problems. Isofrax 1260C Blanket is the product of a long-term research and development effort by Unifrax to produce an insulating blanket which has the high-temperature performance characteristics required in many applications at temperatures up to 2300°F/1260°C and also meets European regulatory requirements (Directive 97/69/EC). Isofrax 1260C Blanket provides low thermal conductivity, excellent thermal stability, thermal shock resistance, low weight, required handling strength, low heat storage, flexibility, and excellent corrosion resistance. Isofrax 1260C Blanket has excellent chemical stability and is unaffected by most chemicals except hydrofluoric and phosphoric acids and concentrated alkalies. If wet by water or steam, thermal and physical properties remain unaffected after drying. Isofrax 1260C Blanket also provides superior resistance to attack from molten aluminum alloys at high temperatures.

    Applications
  • Removable insulating blankets for weld stress relieving
  • Reusable insulation for steam and gas turbines
  • High-temperature kiln and furnace insulation
  • Furnace door linings and seals
  • Furnace repairs
  • Boiler and incinerator linings
  • Seals and gaskets
  • Automotive heat shields
  • Appliance insulation
  • Fire protection
  • Duct, stack and flue linings
  • Vessel covers and lids
  • Personnel heat shields
  • Molten metal splash protection

Information Provided by Unifrax I LLC

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Density
  • Tensile Strength, Yield, ASTM 686-76
  • Tensile Strength, Yield, ASTM 686-76
  • Melting Point
  • Maximum Service Temperature, Air, Recommended Operating Temperature
  • MgO
  • Other, total, Trace Elements
  • SiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Unifrax I LLC

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.