MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
DowAksa CarbonBond™ 200 Slow Adhesive Putty System
Categories: Polymer; Thermoset

Material Notes: User friendly 2:1 by volume mix ratio putty designed for easy mixing and troweling. It can be used to repair / replace broken concrete and bond pre-cured composite reinforcements to concrete substrates. The easy flowing thixotropic putty fills voids and crevasses easily, yet resists sagging even on overhead surfaces. The slow hardener is designed for warm conditions and is excellent for filling large voids and leveling surfaces. The fast hardener is designed to cure at temperatures as low as 10°C. But, it can be used anytime a fast setting putty or adhesive is needed. To facilitate proper mixing and component identification, the Part B slow hardener is Black, and Part B fast hardener is Red. When combined with the White Part A – the putty becomes a light Gray or light Pink respectively. CarbonBond™ 200 Adhesive Putty System is a NSF/ANSI Standard 61 listed product for drinking water systems.

Information provided by DowAksa.

Vendors:
Available Properties
  • Density, Part B
  • Tensile Strength, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Gel Time, 100g
  • Shelf Life, Part A
  • Shelf Life, Part B
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.