Unsaturated polyester resin in styrene, DCPD Appearance: Amber – Opalescent Main resin characteristics: Medium reactivity, Thixotropic Main applications: Pipes and tanks Curing cycle: 16 h at 40°C + 2 h at 90°C (+ 2 h at 120°C for HDT) Information provided by Polynt Composites. |