MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
3M Scotch-Weld™ 4491 Vinyl Bonding Cylinder Spray Adhesive
Categories: Polymer; Adhesive

Material Notes: Industrial grade, high performance, plasticizer resistant bulk spray adhesive formulated for bonding vinyl. The adhesive is available in a convenient, portable, no maintenance aerosol cylinder.

Information provided by 3M

Vendors:
Available Properties
  • Solids Content, aerosol
  • Solids Content, bulk
  • Volatile Organic Compounds (VOC) Content
  • Shear Strength, Overlap, 1/8" Alum/Alum
  • Shear Strength, Overlap, 1/8" Alum/Alum
  • Shear Strength, Overlap, 1/8" Alum/Alum
  • Shear Strength, Overlap, 1/8" Alum/Alum
  • Shear Strength, Overlap, 1/8" Alum/Alum
  • Peel Strength, After 2 week exposure to 71°C, Vinyl-Gerfor NT to Treated plywood, 1 surface Bond
  • Peel Strength, After 2 week exposure to 71°C, Vinyl-Altro to Treated plywood, 1 surface Bond
  • Peel Strength, After 2 week exposure to 71°C, Vinyl-Gerfor MK foamed backed to Composite, 1 surface Bond
  • Peel Strength, After 2 week exposure to 71°C, Vinyl-Gerfor MK foamed backed to Stainless Steel, 1 surface Bond
  • Peel Strength, After 2 week exposure to 71°C, Vinyl-Altro to Composite, 1 surface Bond
  • Peel Strength, After 2 week exposure to 71°C, Vinyl-Altro to Stainless Steel, 1 surface Bond
  • Peel Strength, After 2 week exposure to 71°C, Vinyl-Gerfor MK foamed backed to Treated plywood, 1 surface Bond
  • Peel Strength, After 2 week exposure to 71°C, Vinyl-Altro to Stainless Steel, 2 surface Bond
  • Peel Strength, After 2 week exposure to 71°C, Vinyl-Gerfor NT to Composite, 1 surface Bond
  • Peel Strength, After 2 week exposure to 71°C, Vinyl-Gerfor NT to Stainless Steel, 1 surface Bond
  • Peel Strength, After 2 week exposure to 71°C, Vinyl-Altro to Treated plywood, 2 surface Bond
  • Peel Strength, After 2 week exposure to 71°C, Vinyl-Gerfor MK foamed backed to Stainless Steel, 2 surface Bond
  • Peel Strength, After 2 week exposure to 71°C, Vinyl-Gerfor NT to Treated plywood, 2 surface Bond
  • Peel Strength, After 2 week exposure to 71°C, Vinyl-Gerfor NT to Stainless Steel, 2 surface Bond
  • Peel Strength, After 2 week exposure to 71°C, Vinyl-Altro to Composite, 2 surface Bond
  • Peel Strength, After 2 week exposure to 71°C, Vinyl-Gerfor MK foamed backed to Treated plywood, 2 surface Bond
  • Peel Strength, After 2 week exposure to 71°C, Vinyl-Gerfor NT to Composite, 2 surface Bond
  • Peel Strength, After 2 week exposure to 71°C, Vinyl-Gerfor MK foamed backed to Composite, 2 surface Bond
  • Peel Strength, 180°, Canvas/Steel
  • Peel Strength, 180°, Canvas/Steel
  • Peel Strength, 180°, Canvas/Steel
  • Peel Strength, 180°, Canvas/Steel
  • Peel Strength, 180°, Canvas/Steel
  • Peel Strength, 180°, Canvas/Steel
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.