MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
ChevronTexaco NLGI 0 Ultra Duty Grease EP
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Features

Chevron Ultra-Duty Greases EP are versatile, multipurpose extreme pressure greases with high adhesive propertues designed for a wide variety of automotive and industrial applications.

They are manufactured using selected highly refined, high viscosity base oils, a lithuium-12 hydroxystearate thickener, rust and oxidation inhibitors, and extreme pressure and tackiness additives. They are red in color and stringy in texture.

Chevron Ultra-Duty Greases EP provide thicker shock absorbing oil film protection and greater water resistance than conventional multipurpose greases due to their high viscosity components.

The high viscosity components and tackiness additive give Chevron Ultra-Duty Greases EP an excellent adhesive quality which provides a tenacious lubricating film in working parts. The lubricants stay in place under severe abrasive operating conditions to resist water washout and shock load wear.

The outstanding tackiness characteristics of Chevron Ultra-Duty Greases EP make these products somewhat harder to pump than the historical soft, buttery greases. For this reason, we recommend the use of a heavy follower play with air driven grease pumps.

Chevron Ultra-Duty Greases EP lubricate well at low temperatures. The ASTM D 1478 low temperature torque test shows that they retain their lubricating capacity, as defined by military specification MIL-G-81322, sown to about -26°C (-15°F).

Applications

Chevron Ultra-Duty Greases EP are recommended for use in automotive and industrial equipment operating under severe service except were very high operating temperatures are encountered. Typical application are: mining equipment, construction equipment, material handling equipment, marine deck equipment, amine deck cranes, oil filed equipment, offshore drilling equipment, paper machines, dredging equipment, logging equipment, rock quarry equipment, etc., operating in water, mud, or dusty conditions.

Chevron Ultra-Duty Greases EP will provide the needed shock load and rust protection and, best of all, they stay put which means less frequent regreasing. They are not our primary recommendation for high temperature wheel bearings. Chevron Delo® Greases EP, Chevron RPM® Automotive LC Greases EP, or Chevron Black Pearl® Greases EP are preferred for wheel bearing applications

In industrial service, Chevron Ultra-Duty Greases EP are recommended for use in all types of plain and antifriction bearings from 1-1/2 inch OD to over 16 inch OD, operating at speeds from 50 to 3000 rpm, as well as slides, gears, ways, etc.

Key Words: CPS Number: 238013; MSDS Number: 6790
Vendors:
Available Properties
  • Viscosity Measurement, ASTM D2270, Viscosity Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Kinematic Viscosity at 100°C (212°F), ASTM D445
  • Four Ball Extreme Pressure, Weld Load, Weld Point
  • Penetration, Worked
  • Penetration P(0), 1/10 mm
  • Timken Test
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Flash Point, ASTM D92
  • Dropping Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.