Hostacom 68F4-3 BLK fractional melt flow, 3,400 MPa flexural modulus, 30% talc-filled, blow molding and extrusion grade polypropylene homopolymer is typically used for applications that require high strength, stiffness, impact resistance and processability. Applications: Panels & Profiles.Information provided by LyondellBasell. |