MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Tipco Clearbatch - 10 Clarifying & Nucleating Masterbatch
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Description: Clearbatch-10 is Tipco's Advanced Clarifying & Nucleating Masterbatch based on Polypropylene (PP) containing 10% of special proprietary additive that influences the Crystallization Kinetics of PP. It is suitable for Indirect Food Contact use & in Odor Sensitive PP Products that require high Clarity, Gloss & Stiffness. Polypropylene with Clearbatch-10 is called Clarified PP.

Applications: Clearbatch-10 is added to Polypropylene for a variety of end-use applications such as:

  • Thermoforming of cups, Trays, Transparent Panels, Containers
  • Injection Stretch Blow Molding of Bottles & Containers for packing Medicine, Baby Foods, etc.
  • Thin Walled Injection Moldings, Clear/Translucent Films, Sheets, Profiles & various Extruded Sections

Information provided by the Manufacturer, Tipco Industries Ltd., India.

Vendors:
Available Properties
  • Haze, ASTM D1003, Random Copolymer with 2%-2.25% Clearbatch-10 versus 65% without Clearbatch-10
  • Haze, ASTM D1003, Homopolymer with 2%-2.25% Clearbatch-10 versus haze of 71% without Clearbatch-10
  • Gloss, ASTM D523, Homopolymer with between 2%-2.25% Clearbatch-10 versus gloss of 93% without Clearbatch-10
  • Gloss, ASTM D523, Random Copolymer with between 2%-2.25% Clearbatch-10 versus gloss of 93.9% without Clearbatch-10
  • Yellow Index, ASTM E313, Homopolymer with between 2%-2.25% Clearbatch-10 versus yellow index of 1.58 without Clearbatch-10
  • Yellow Index, ASTM E313, Random Copolymer with between 2%-2.25% Clearbatch-10 versus yellow index of 1.61 without Clearbatch-10
  • Transmission, Visible, transparent; thickness not quantified
  • Processing Temperature, Unless plate out occurs.
  • Melt Temperature
  • Mold Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Tipco Industries Ltd., India

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.