MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
SABIC SABIC® PP FPC70 PP (Global)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: As part of SABIC® PP FLOWPACT portfolio, FPC70 delivers high top load performance (potential downgauging) with a superior stiffness / impact balance. It is nucleated and has good antistatic performance with easy demoulding. This grade has good flow behavior, and it is typically used by our customer for high-speed injection moulding process, potentially enabling very cost efficient processing on the basis of easy mould filling and very short cycle times. Applications: SABIC® PP FPC70 is typically used in rigid packaging applications for both food and non-food industries. This includes packaging for yellow fats, cheese spreads, dairy, frozen, chilled and ambient food, household chemicals and paints among others. It can be also used in several applications in the caps & closures as well in housewares. The grade has excellent heat deflection temperature making it may particularly be used for hot fill applications. This product is not intended for and must not be used in any pharmaceutical/medical applications.

Information provided by SABIC

Vendors:
Available Properties
  • Density, ASTM D1505
  • Melt Flow, ISO 1133
  • Tensile Strength, Yield, ISO 527-2 1A, Speed of testing: 50 mm/min
  • Elongation at Yield, ISO 527-2 1A
  • Tensile Modulus, ISO 527-2 1A, Speed of testing: 1 mm/min
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Charpy Impact, Notched, ISO 179/1eA
  • Charpy Impact, Notched, ISO 179/1eA
  • Charpy Impact, Notched, ISO 179/1eA
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75, Flat wise (testbar 80*10*4mm)
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75, Flat wise (testbar 80*10*4mm)
  • Vicat Softening Point, ISO 306, at 50 N (VST/B); Temperature rate: 120ºC/h
  • Vicat Softening Point, ISO 306, at 10 N (VST/A); Temperature rate: 120ºC/h
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.