MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
LATI Latene® AG3H2W G/30-V0 30% Glass Fiber with Chemical Bond, Heat-Stabilized Polypropylene Homopolymer (PPH)  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Description: Latene series thermoplastics are polypropylene homopolymer (PPH) products. They provide good mechanical, thermal and electrical properties together with good chemical inertness. The wide range of filled Latene allows a choice based on shrinkage, impact resistance, rigidity and/or surface finish, according to project demands. Compared to filled versions, reinforced Latene grades, especially chemically coupled versions, offer considerably greater rigidity and thermal resistance under loads. All the Latene grades may be adapted to specific project needs. Several characteristics may be enhanced, such as flowability, heat-stability, anti-static quality, stability on contact with metals and detergents, UV-stabilization (except for normal self-extinguishing types).

Specific Notes for this Material: self-extinguishing UL94 V0 with halogens; stabilized for heat and contact with metals; 30% glass fiber with chemical bond; good rigidity; good mechanical characteristics.

Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.

All data provided by LATI.

Vendors:
Available Properties
  • Density, ISO 1183
  • Water Absorption, ISO 62, at 23°C
  • Linear Mold Shrinkage, LATI
  • Linear Mold Shrinkage, Transverse, LATI
  • Melt Flow, ISO 1133
  • Hardness, Rockwell M, ASTM D785
  • Tensile Strength, Ultimate, ISO 527
  • Tensile Strength, Ultimate, ISO 527
  • Tensile Strength, Ultimate, ISO 527
  • Tensile Strength, Ultimate, ISO 527
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D256
  • Charpy Impact Unnotched, DIN 53453
  • Charpy Impact Unnotched, DIN 53453
  • Charpy Impact Unnotched, DIN 53453
  • Dielectric Strength, IEC 243-1
  • Comparative Tracking Index, IEC 112
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Vicat Softening Point, ISO 306, 50°C/h 50N
  • Flammability, UL94
  • Flammability, UL94
  • Oxygen Index, ISO 4589
  • Glow Wire Test, IEC 695-2-1
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature, Non-reinforced self-extinguishing types; can be reduced with vacuum oven.
  • Dry Time, Non-reinforced self-extinguishing types; can be reduced with vacuum oven.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.