MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
INEOS Styrolution K-Resin® DK11E SBC
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Product Description: K-Resin® DK11E makes a clear, stiff, very tough, high gloss film suitable for applications such as candy twist wrap, shrink sleeves and overwrap. K-Resin® K-Resin® SBC grade designed for blown film extrusion is DK11E.
Features: Excellent Clarity; High Surface Gloss; Good Heat Sealability
Applications: Medical Packaging; Produce Packaging; Twist Wrap; Lidstock and Labeling Film

Availability: Latin America; North America

Features: Block Copolymer; Good Stiffness; Good Toughness; Heat Sealable; High Clarity; High Gloss

Uses: Film; Food Packaging; Labels; Medical Packaging; Packaging

Appearance: Clear/Transparent

Form: Pellets

Processing Method: Blown Film; Extrusion; Film Extrusion

Information provided by INEOS Styrolution

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Vapor Transmission, ASTM F1249, 0% to 85% RH gradient
  • Oxygen Transmission Rate, ASTM D3985, 0% RH
  • Melt Flow, ASTM D1238
  • Film Tensile Strength at Yield, MD, ASTM D882
  • Film Tensile Strength at Yield, TD, ASTM D882
  • Film Elongation at Break, MD, ASTM D882
  • Film Elongation at Break, TD, ASTM D882
  • 1% Secant Modulus, ASTM D882, TD
  • 1% Secant Modulus, ASTM D882, MD
  • Dart Drop, Total Energy, ASTM D3763, Peak Force
  • Elmendorf Tear Strength MD, ASTM D1922
  • Elmendorf Tear Strength TD, ASTM D1922
  • Dart Drop Test, ASTM D1709
  • Vicat Softening Point, ASTM D1525, Rate B (120°C/h), Loading 1 (10 N)
  • Haze, ASTM D1003
  • Gloss, ASTM D2457, mold temperature 100°F
  • Transmission, Visible, ASTM D1003
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.