MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Chevron Phillips Ryton® R-7-220NA Polyphenylene Sulfide Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or repeated exposure to high temperature water.

Measured on 102mm x 102mm x 3.2 mm plaques, edge gated.

Information provided by Chevron Phillips

Solvay Specialty Polymers has acquired the Ryton product line. This product was discontinued prior to the acquisition and is listed under the Chevron Phillips name for historical purposes.

Vendors:
Available Properties
  • Density, ISO 1183A
  • Water Absorption, ASTM D-570
  • Linear Mold Shrinkage, Flow
  • Linear Mold Shrinkage, Transverse
  • Tensile Strength, Yield, ISO 527
  • Elongation at Yield, ISO 527
  • Flexural Strength, ISO 178
  • Flexural Modulus, ISO 178
  • Compressive Strength, ISO 604
  • Izod Impact, Notched (ISO), ISO 180A
  • Izod Impact, Unnotched (ISO), ISO 180A
  • Volume Resistivity, ASTM D-257
  • Dielectric Constant, ASTM D-150
  • Dielectric Constant, ASTM D-150
  • Dielectric Strength, ASTM D-149
  • Dissipation Factor, ASTM D-150
  • Dissipation Factor, ASTM D-150
  • Arc Resistance, ASTM D-495
  • CTE, linear, ISO 11359-2, Axial
  • CTE, linear, ISO 11359-2, Axial
  • CTE, linear, Transverse to Flow, ISO 11359-2
  • CTE, linear, Transverse to Flow, ISO 11359-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75
  • Flammability, UL94
  • Melt Temperature
  • Mold Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Chevron Phillips Chemical Company LP; ChevronPhillips

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.