MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Chevron Phillips Marlex® K306 Fully Formulated Medium Density Hexene Copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Extruded

Material Notes: Fully Formulated Medium Density Hexene Copolymer

Customer Benefits: This extrusion grade hexene copolymer has good processability, excellent melt strength, broad fusion range, outstanding ESCR, meets the requirements of GRI-GM12

Applications: Recommended rein for pond liners, gas and chemical tank containment liners, landfill liners.

Processing Recommendations:
Extrusion Melt Temperature: Upper Limit: 232°C, Lower Limit: 193°C

Specification Data: ASTM D1248 - Type III, Class A, Category 5. ASTM D4976-89 PE 225

Data provided by Chevron Phillips Chemical Company, LP.

Vendors:
Available Properties
  • Density, ASTM D1505
  • ESCR 100% Igepal®, Condition C, F50, ASTM D1693
  • ESCR 10% Igepal®, Condition B, F50, ASTM D1693
  • Melt Flow, Condition 190/2.16; ASTM D1238
  • Tensile Strength, Yield, 2 in per min; ASTM D638 Type IV
  • Elongation at Break, 2 in per min; ASTM D638 Type IV
  • Flexural Modulus, ASTM D790
  • Processing Temperature, Extrusion
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Chevron Phillips Chemical Company LP; ChevronPhillips

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.