Temper: Mill-hardened Temper, TM - 1/2 Hard Fabrication Properties: Excellent Suitability – Soldering, Brazing, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Good Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding Common Fabrication Processes: Forming and Bending; Stamping Typical uses: Connectors; Leadframe Sockets Applicable Specifications: Sheet & Strip – ASTM B422/B422M; Strip – ASTM B888/B88M |