MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Go Yen Chemical GYC-Nano Self-Cleaning Coating
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro: GO YEN CHEMICAL CO., LTD. is the largest manufacturer of specialty chemicals in Taiwan. We devote ourselves to supplying products with superior quality and innovative solutions to our customers to satisfy the market needs. GYC-Nano Self-Cleaning Coating is a nano coating which offers exceptional antibacterial property and self-cleaning functionality. With strengthened weather resistance and structural reinforcement, the nano coating features high water resistance, acid/alkali resistance, and wear resistance that provides outstanding aging resistance and dirt resistance that is especially suited for indoor wall.

Advantages:

  • Provides excellent self-cleaning functionality
  • Provides excellent dirt resistance due to its nano structure
  • Provides high water resistance, acid/alkali resistance
  • Provides high wear resistance
  • Provides outstanding aging resistance and dirt resistance.
  • Compatible with various paints and coatings

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • Density
  • pH
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.