MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
ExxonMobil Vistamaxx™ 3980FL Propylene-based Elastomer - High Purity, Low Gel
Categories: Polymer; Film; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO), Film Grade

Material Notes: Product Description: Vistamaxx 3980FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution. It is produced using ExxonMobil Chemical's EXXPOL™ Catalyst Technology. The "FL" designates this is a high purity grade with very low gel content, making it suitable for premium and performance film and molding applications.

Key Features:

  • Suitable for a wide range of cast and blown film, molding and various polymer modification and compounding applications.
  • Can be blended with PP, PE and other polyolefins for softening, stress-whitening and impact improvement.
  • Excellent adhesion to conventional and metallocene PP and PE for exceptional extrusion coating, lamination and tie-layer performance.
  • Very low seal initiation temperature combined with high seal strength when used as a sealing layer of co-extruded structures.
  • Good optical properties.
  • Good chemical resistance to aqueous systems and non-hydrocarbon based fluids.
  • May be used in food contact applications (with some restrictions).
  • EU and China RoHS compliant.
Applications:
  • Blown Film
  • Polymer Modification
  • Compounding
  • Cast Film
  • Molding
Uses:
  • Compounding
  • Film
  • Packaging
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical.

Vendors:
Available Properties
  • Specific Gravity, ASTM D1505
  • Melt Flow, ExxonMobil Method, melt flow rate
  • Melt Flow, ExxonMobil Method
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, Yield, ASTM D412
  • Tensile Stress at Strain, ASTM D412
  • Tensile Stress at Strain, ASTM D412
  • Elongation at Yield, ASTM D412
  • Flexural Modulus, 1% Secant, ASTM D790
  • Tear Strength, ASTM D624, Die C
  • Tensile Set, ASTM D412
  • Vicat Softening Point, ASTM D1525
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Exxon Chemical

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.