Structural Adhesives for Rugged Bonding, Sealing, Tacking and Potting in Seconds Multi-Cure® 600 Series products are rapid setting adhesives that cure by UV light, activator or heat. These products form structural strength bonds to glass, metal and many filled plastic substrates in seconds.
Dymax 602 Structural Adhesive Key Substrates: Polycarbonate (primary), Styrene, Acrylic, Metal Typical Use: Armature wire strain relief; structural metal bonds; E-coat |