MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
ChevronTexaco ParaLux™ 2401 Paraffinic Process Oil
Categories: Fluid; Lubricant

Material Notes: Features

PARALUX is produced using an all-hydroprocessing route which transforms the molecular structure of undesirable aromatics into highly desirable saturates. This produces a process oil with superior physical and chemical properties :

  • lower aromatics result in superior color stability.
  • Lower volatility improves efficiency.
  • Excellent compatibility with rubber polymers reduces processing headaches.

Applications

Because PARALUX is produced by all-hydroprocessing, it has performance properties that surpass most conventional paraffinic process oils and approach or surpass many of the performance characteristics of technical white oils. These advantages include:

  • Exceptionally low aromatic content
  • Better color and UV stability than conventional paraffinic or naphthenic oils
  • Almost complete resistance to degradation from ultraviolet discoloration
  • Lower volatility results in fewer emissions, so less make-up oil is needed and costs are minimized
  • Excellent compatibility with rubber polymers which require paraffinic oils. Only all-hydroprocessed oils can deliver all of these advantages

Chevron ParaLux Process Oils are ideal for use in compounding a wide variety of products, including :

  • Footwear
  • Agricultural Spray
  • Furniture Polish
  • Textiles
  • Wire and Cable insulation
  • Adhesives, sealants and coatings
  • Polymer modified asphalts
  • Asphalt extender
  • Automobile interior moldings
  • Automotive under hood parts
  • Tires, tire whitewalls, tubes, and inner liners
  • Insulation
  • Gels
  • Dielectric Fluids
  • Drilling Fluids
  • Carpet Underlayment
  • Heat transfer fluids
  • Foam
  • Household products
  • Roofing compounds
  • Rubber membranes
  • Weather Stripping

Key Words: CPS Number: 240674; MSDS Number: 7022
Vendors:
Available Properties
  • Specific Gravity
  • API Gravity
  • Viscosity Measurement, Viscosity Gravity Constant
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Kinematic Viscosity at 100°C (212°F), ASTM D445
  • Pour Point, ASTM D97
  • Flash Point, ASTM D92
  • Refractive Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.