MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Evonik ULTRASIL® 5000 GR Silicon dioxide
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: ULTRASIL 5000 GR is a mechanically compacted granulate. On account of the granulation process it leads to less dust development during mixing. ULTRASIL 5000 GR is a highly dispersible and reinforcing silica with a specific surface area of approximately 120 m2/g. Compared to standard silicas with a specific surface area of approximately 160 m2/g. ULTRASIL 5000 GR provides lower compound viscosities, ie an improved processing behavior at equal loading. Furthermore, lower dynamic stiffness at low ambient temperatures and improved rolling resistance are achieved for tire tread compounds. Higher silica loadings will improve wet traction properties and allow to optimize winter properties. Bifuctional organosilanes like Si 69®, Si 79®, Si 266® or VP Si 363® are required for the use of ULTRASIL 5000 GR in tired tread compounds. The use of diethylen glycol, triethanolamine or other alkaline accelerators might be necessary in order to achieve optimum in-rubber data. Application fields are: Tires, mechanical rubber goods.

Information provided by Evonik

Vendors:
Available Properties
  • Density, ASTM D1513, Pour density
  • pH, ISO 787-9, 5% in water
  • Specific Surface Area, ISO 5794-1G, CTAB
  • Specific Surface Area, ISO 9277, N2
  • SiO2, ISO 3262-19
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.