MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Trinseo EMERGE™ PC/PET 9500CR SK PC/PET
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend

Material Notes: Product Description: EMERGE™ PC/PET 9500CR SK advanced resin is a polycarbonate blend with excellent chemical and ignition resistance properties. This grade has been tested to ISO 10993 Parts 5 & 10 and is suitable for skin contact applications. It is designed for use in medical equipment housings and other applications that are subject to repeated exposure to a variety of cleaners and disinfectants commonly used in hospitals. This grade has good aesthetics and excellent toughness. It has a UL 94 rating of V0 at 2.0 mm.
Main Characteristics: Excellent chemical resistance; UL listing for V0 and 5V; Tested under ISO 10993 (Parts 5 & 10)
Applications: Medical device housings or enclosures

Availability: Asia Pacific; Europe; North America

Features: Chemical Resistant; Flame Retardant; Good ESCR (Stress Crack Resist.); Good Toughness; Ignition Resistant; Pleasing Surface Appearance; UV Stabilized

Uses: Electrical Housing; Housings; Medical Device Housings; Medical Devices; Medical/Healthcare Applications

RoSH Compliance: RoSH Compliant

Appearance: Colors Available; Opaque

Form: Pellets

Processing Method: Injection Molding

Information provided by Trinseo

Vendors:
Available Properties
  • Density, ASTM D792
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Linear Mold Shrinkage, Transverse, ASTM D955
  • Melt Flow, ASTM D1238
  • Melt Flow, ASTM D1238
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength at Break, ASTM D638, 2.0 in/min
  • Tensile Strength, Yield, ISO 527-2/50
  • Tensile Strength, Yield, ASTM D638, 2.0 in/min
  • Tensile Modulus, ASTM D638, 0.039 in/min
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Dart Drop, Total Energy, ASTM D3763, Peak
  • Dart Drop, Total Energy, ASTM D3763, Peak
  • Dart Drop, Total Energy, ASTM D3763, Total
  • Dart Drop, Total Energy, ASTM D3763, Total
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243-1, in Oil
  • Dielectric Strength, IEC 60243-1, in Oil
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • CTE, linear, Parallel to Flow, ASTM D696
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Unannealed
  • Vicat Softening Point, ASTM D1525, Rate B (120°C/h), Loading 1 (10 N)
  • Vicat Softening Point, ISO 306/A120
  • Flammability, UL94
  • Flammability, UL94
  • Flammability, UL94
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Trinseo, former Styron

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.