MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Ineos R08G-01 PP Random Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Molded

Material Notes: Product Description: R08G-01 is a random copolymer polypropylene for film, blow molding, expanded PP foam beads, and injection molding applications with a barefoot additive package.
Availability: North America
Additive: Slip
Features: Food Contact Acceptable; Random Copolymer; Slip
Uses: Blow Molding Applications; Film; Foam
Agency Rating: EC 1907/2006 (REACH); FDA 21 CFR 177.1520
RoHS Compliance: Contact Manufacture
Forms: Pellets
Processing Method: Blow Molding; Film Extrusion; Foam Processing; Injection Molding

Information provided by INEOS Olefins & Polymers USA

Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Flow, ASTM D1238
  • Hardness, Rockwell R, ASTM D785, Injection Molded
  • Tensile Strength at Break, ASTM D638, 2.0 in/min, Injection Molded
  • Tensile Strength, Yield, ASTM D638, 2.0 in/min, Injection Molded
  • Elongation at Break, ASTM D638, 2.0 in/min, Injection Molded
  • Elongation at Yield, ASTM D638, 2.0 in/min, Injection Molded
  • Flexural Modulus, 1% Secant, ASTM D790A, Injection Molded
  • Izod Impact, Notched, ASTM D256, Injection Molded
  • Izod Impact, Notched, ASTM D256, Injection Molded
  • Izod Impact, Notched (ISO), ASTM D256, Area, Injection Molded
  • Izod Impact, Notched (ISO), ASTM D256, Area, Injection Molded
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Unannealed, Injection Molded
  • Vicat Softening Point, ASTM D1525
  • Haze, ASTM D1003
  • Gloss, ASTM D2457, 60°, Injection Molded
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Ineos Olefins & Polymers USA

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.