MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Geon® Performance Solutions FIT E 50 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Geon® FIT E 50 is a low molecular weight homopolymer resin intended for use as a Formulation Improvement Tool (FIT) in plastisol formulations which enhance the plastisol usage (pot life) and reduce the viscosity aging characteristics. Geon® FIT E 50 resins increase physical properties up to 30% compared to traditional blending resins. It allows the addition of up to 40phr of filler, significantly decreasing the formulation cost. It improves air release properties, provides faster de -aeration time and reduces scrap rates caused by the presence of air bubbles or voids in finished part. This resin reduces the viscosity profile of the plastisol providing an improved 'ease of coating' performance resulting a more uniform plastisol coating and improving line up time. Geon® FIT E 50 is recommeded for solid and foamed plastisol applications for instance coated fabrics and carpet tiles, cast films and coatings, rotational and slush molded parts, dip molded and coated parts, and walk off and foam mats and pads.

Note: The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Geon® ALTC (formulation): 60phr Geon® 121A, 40phr Geon® FIT E 50, 57phr DINP, 3phr ESO, and 2phr Therm-Chek SP 120 LOHF Geon® STP 1203(formulation): 60phr Geon® 178, 40phr Geon® FIT E 50,and 60phr DOP

Geon Performance Solutions was created from PolyOne in 2019.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Volatiles, Internal Method, Geon® STP 1242
  • Apparent Bulk Density, Internal Method, Geon® STP 1169
  • Particle Size, Internal Method, Geon® DFT 1466
  • Particle Size, Internal Method, 95%; Geon® DFT 1466
  • Particle Size, Internal Method, 99%; Geon® DFT 1466
  • Relative Viscosity, Internal Method, Correlation, Cyclohexanone 1%
  • Brookfield Viscosity, Internal Method, Initial Viscosity @ 20 rpm; Geon® ALTC 22 (with provided formulation)
  • Brookfield Viscosity, Internal Method, Initial Viscosity @ 2 rpm; Geon® ALTC 22 (with provided formulation)
  • Brookfield Viscosity, Internal Method, One Day Viscosity @ 2 rpm; Geon® ALTC 22 (with provided formulation)
  • Brookfield Viscosity, Internal Method, One Day Viscosity @ 20 rpm; Geon® ALTC 22 (with provided formulation)
  • Viscosity Measurement, ASTM D1243-60-A, Inherent
  • Melt Flow, Internal Method, Severs Efflux; Geon® ALTC 23 (with provided formulation)
  • Haze, Internal Method, Fused 5 mins @ 350F Geon® ALTC 66 (with provided formulation)
  • Gloss, Internal Method, 60 Degree Fused 5 mins @ 350 F Geon® ALTC 65 (with provided formulation)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.