Tough, rubber-like urethane compound for making a broad range of repairs, and for tooling and molding applications. Uses: Repair and rebuild conveyor belts; seal electrical cables; seal woven fabric belting from wear and abrasion; fill expansion/control joints; pot and encapsulate parts. Features: Excellent humidity resistance, High tensile and tear strength, Easy-to-use 400 ml cartridge, Fast-curing; self-leveling, Oil-resistant.Information provided by ITW Performance Polymers. |