Temper: Mill-hardened Temper, TM - Hard Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked; Good Suitability – Gas Shielded Arc Welding; Fair Suitability – Spot Weld, Seam Weld, Butt Weld, Capacity for Being Hot Formed Typical Uses: Automotive Electronic Connectors; Connectors, Automotive; Connectors, Terminals, Contact Springs, Fuse Clamps, Circuit breaker components |