MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Neutrex Purgex™ 456 Plus Purging Compound
Categories: Polymer; Thermoplastic; Purging Compound

Material Notes: Blend, polyethylene, and FDA-approved active component. Non-toxic, non-abrasive, and safe. Ready to use and easy to remove.

PURGEX 456 Plus is used for color and/or material changes and the removal of residual contamination in thermoplastic injection molding, extrusion, or blow molding equipment. PURGEX 456 Plus will efficiently purgehe barrel, screw, and nozzle, as well as hot runners. This blend removes all types of colorants and commodity resins, including polypropylene, polyethylene, and their copolymers. PURGEX 456 Plus is used to neutralize HCl gasses in PVC purging applications. PURGEX 456 Plus assures rapid turnaround on color and material changes with polyolefins and their copolymers, styrenics polymers, acetals, vinyls, TPO, TPU, and many more resins processed in this temperature range.

Key Words: Purge
Vendors:
Available Properties
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Neutrex, Inc

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.