MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Kohesi Bond KB 1061 Rapid curing, two component epoxy for bonding and sealing
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Product Highlights:
  • Very rapid curing; “5 minute” type epoxy
  • Excellent flow properties
  • Convenient mixing ratio
  • Outstanding electrical insulation properties
  • Exceptional physical strength properties
  • Stellar dimensional stability
Kohesi Bond KB 1061 is a two component, “5 minute curing” type epoxy system suitable for bonding and sealing applications. It has an easy 1:1 (Part A: Part B) mix ratio by weight or volume. It is important to explain the common misapprehension on “5 minute” epoxy systems. In actuality, the working life is around 5 minutes; the real set up time can range from 10-20 minutes depending on the actual application and cure conditions. Based on these conditions, complete cure can range from 12-18 hours. It readily cures at room temperature and can achieve faster cures at elevated temperatures. KB 1061 offers an extensive service temperature range of 4K (-269.15°C) to +120°C. This adhesive fosters outstanding physical strength properties as well as dimensional stability. It offers minimal shrinkage upon cure and good chemical resistance properties. KB 1061 adheres well to a wide variety of substrates including metals, composites, ceramics, most plastics and glass. Upon polymerization KB 1061 offers typical epoxy type superior electrical insulation. Part A is clear in color and Part B is amber in color. KB 1061 is widely used in electronics, medical, food, aerospace and specialty OEM industries. It is also useful for prototyping and repair situations, where faster cure is desirable.

Typical Applications:

  • Bonding
  • Sealing

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors:
Available Properties
  • Density, Part B
  • Density, Part A
  • Viscosity, Part A
  • Viscosity, Part B
  • Hardness, Shore D
  • Tensile Strength
  • Tensile Modulus
  • Adhesive Bond Strength, Tensile Lap Shear, Al/Al
  • Volume Resistivity
  • Dielectric Constant
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Option 2
  • Cure Time, Option 1
  • Working Life, 100 g of mixed epoxy
  • Shelf Life, in original unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Ensinger PEI
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.