MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Westlake EBAC® SP1806 17.5%, Ethylene-Methyl Acrylate Copolymer
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Description: Westlake EBAC® SP1806 is an ethylene butyl acrylate copolymer designed for extrusion coating and laminating. SP1806 can also be compounded as an impact modifier or used in highly filled applications. Westlake EBAC® resins are less crystalline and softer than polyethylene and offer compatibility and adhesion to typically difficult to bond to polymers. SP1806 is non-corrosive at extrusion temperatures and has excellent thermal stability.
    Key Attributes:
  • Good adhesion/compatibility to various substrates
  • Good heat and RF sealing
  • Low temperature toughness
  • Soft, flexible, tough without plasticizer
    Application/Uses:
  • Extrusion coating / laminations
  • Flexible Packaging
  • Impact Modifier
  • Compounding / high filler loadings

Information provided by Westlake Chemical

Key Words: Good adhesion/compatibility to various substrates
Vendors:
Available Properties
  • Density, ASTM D1505
  • Butyl Acrylate Content, Westlake
  • Melt Flow, ASTM D1238
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength at Break, ASTM D 638 Type IV Specimen, 50 mm/min
  • Elongation at Break, ASTM D 638 Type IV Specimen, 50 mm/min
  • Melting Point, ASTM D3418, by DSC
  • Vicat Softening Point, ASTM D1525
  • Brittleness Temperature, ASTM D746
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Westlake Chemical Corporation

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.