MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Covestro MAKROFOL® UV 503 9-2 060004 Polycarbonate Film
Categories: Polymer; Film; Thermoplastic; Polycarbonate (PC)

Material Notes: Makrofol UV 244 6-2 040004 is an coextruded film based on Makrolon® polycarbonate.

Properties / Applications: Makrofol UV 503 9-2 060004 comprises good light dispersion properties with all of the well known advantages of polycarbonate, such as excellent mechanical and optical properties. Typical application is automotive lighting. Makrofol UV 503 9-2 060004 is available in 0.010 ” to 0.030 ” (250 to 750 microns) standard thickness. Other thicknesses are available on request. The surface finish of Makrofol UV 503 9-2 060004 is velvet/very fine matte.

Information provided by Covestro

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Linear Mold Shrinkage, Flow, IEC 60674-2
  • Linear Mold Shrinkage, Transverse, IEC 60674-2
  • Tensile Strength at Break, ASTM D882
  • Tensile Strength, Yield, ASTM D882
  • Elongation at Break, ASTM D882
  • Flexural Modulus, ASTM D790
  • Tear Strength, ASTM D1004
  • CTE, linear, Parallel to Flow, DIN 53752
  • CTE, linear, Transverse to Flow, DIN 53752
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Vicat Softening Point, ASTM D1525, Rate A
  • Gloss, ASTM D2457, 60° top side black inked second surface
  • Transmission, Visible, ASTM D1003
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Covestro Deutschland AG, Bayer MaterialScience

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.