Available Properties |
---|
- Volatiles
- Outgassing - Total Mass Loss, TWL
- Collected Volatile Condensable Material
- Storage Temperature
- Tensile Strength, Flatwise
- Tensile Strength, Flatwise
- Tensile Strength, Flatwise
- Tensile Strength, Flatwise
- Tensile Strength, Flatwise
- Shear Strength, Lap, Bonded Exposure: 30 days at 160°F (71°C), 100% RH, 100% Cohesive Failure
- Shear Strength, Lap, Precured Composite Substrate: PEEK (APC™-2)
- Shear Strength, ASTM D1002, Lap
- Shear Strength, Lap, Baseline
- Shear Strength, Lap, 85% Adhesive Failure, 15% cohesive Failure
- Shear Strength, Lap, 70% Cohesive Failure, 30% Laminate Failure
- Shear Strength, Lap, 60% Cohesive Failure, 40% Laminate Failure
- Shear Strength, Lap, Bonded Exposure: 30 days at 160°F (71°C), 100% RH, 50% Cohesive Failure, 50% Laminate Failure
- Shear Strength, Lap, Bonded Exposure: 30 days at 160°F (71°C), 100% RH, 100% Laminate Failure
- Shear Strength, Lap, Precured Composite Substrate: PEEK (APC™-2)
- Shear Strength, Lap, wet, Precured Composite Substrate: PEEK (APC™-2)
- Shear Strength, Lap, Precured Composite Substrate: PEEK (APC™-2)
- Shear Strength, ASTM D1002, Lap
- Shear Strength, Lap, Baseline
- Shear Strength, Lap, Cure Cycle 60 minutes 350°F (177°C)
- Shear Strength, ASTM D1002, Lap
- Shear Strength, Lap, Cure Cycle 90 minutes 250°F (121°C)
- Shear Strength, Lap, Cure Cycle 60 minutes 300°F (149°C)
- Shear Strength, ASTM D1002, Lap
- Shear Strength, Lap, Baseline
- Shear Strength, ASTM D1002, Lap
- Shear Strength, Lap, Cure Cycle 90 minutes 250°F (121°C)
- Shear Strength, Lap, Cure Cycle 60 minutes 350°F (177°C)
- Shear Strength, Lap, Cure Cycle 60 minutes 300°F (149°C)
- Peel Strength, Floating Roller
- Peel Strength, Floating Roller, Cure Cycle 90 minutes 250°F (121°C)
- Peel Strength, Floating Roller, Cure Cycle 60 minutes 300°F (149°C)
- Peel Strength, Floating Roller, Cure Cycle 60 minutes 350°F (177°C)
- Peel Strength, Floating Roller, Bonded Exposure: 30 days at 160F (71C), 100% RH
- Peel Strength, Floating Roller, Pre-Bond Film Exposure:15 days at 75°F (24°C), 80% RH, Bonded Exposure: 30 days at 160°F (71°C), 100% RH
- Peel Strength, Floating Roller, Pre-Bond Film Exposure
- Peel Strength, Floating Roller, Pre-Bond Film Exposure
- Peel Strength, Floating Roller, Pre-Bond Film Exposure:15 days at 75°F (24°C), 80% RH
- Peel Strength, Floating Roller, Bonded Exposure: 30 days at 160F (71C), 100% RH
- Peel Strength, Floating Roller, Pre-Bond Film Exposure:15 days at 75°F (24°C), 80% RH, Bonded Exposure: 30 days at 160°F (71°C), 100% RH
- Peel Strength, Floating Roller, Pre-Bond Film Exposure:15 days at 75°F (24°C), 80% RH
- Peel Strength, Floating Roller, Cure Cycle 90 minutes 250°F (121°C)
- Peel Strength, Floating Roller, Cure Cycle 60 minutes 300°F (149°C)
- Peel Strength, Floating Roller, Cure Cycle 60 minutes 350°F (177°C)
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Glass Transition Temp, Tg, Lap, Cure Cycle 60 minutes 300°F (149°C)
- Glass Transition Temp, Tg, Lap, Cure Cycle 60 minutes 350°F (177°C)
- Glass Transition Temp, Tg, Lap, Cure Cycle 90 minutes 250°F (121°C)
- Glass Transition Temp, Tg
- Shelf Life
|
| | |