MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Trinseo MAGNUM™ 3904 Acrylonitrile Butadiene Styrene (ABS) Resin
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: MAGNUM™ 3904 is a medium heat ABS. Its very high impact properties make it suitable for main interior automotive applications. MAGNUM ™ 3904 is available in Europe and China, locally produced in major car production regions. Due to its excellent extrusion capabilities, this product is also used for large thermoformed parts, for Truck and Bus applications.

Benefits:

  • Lot to lot consistency allowing for optimal machine parameters setting from the start
  • Self-coloring enabling improvement of costs by using less pigments and lowering your logistic costs
  • Low VOC allowing a better interior air quality facing increasing regulatory and OEMs constraints
  • Heat stability during wide range of processing temperatures: enhanced part design freedom
  • Contains low amounts of gel providing for excellent thermoformability with low levels of scrap
Applications:
  • Main interior automotive applications requiring high impact
  • Various interior trims, under the beltline
  • Large sized applications in commercial transportation
Automotive Specifications:
  • BMW GS 93016
  • GM QK 002022 Color: Natural
  • DAIMLER DBL 5404.03
  • VAG VW-TL 527

Information provided by Trinseo.

Vendors:
Available Properties
  • Density, ISO 1183/B
  • Apparent Bulk Density, ISO 60
  • Linear Mold Shrinkage, Flow, ISO 294-4
  • Melt Flow, ISO 1133
  • Tensile Strength, Yield, ISO 527-2/50, Injection Molded
  • Tensile Strength, Yield, ISO 527-2/100, Injection Molded
  • Elongation at Yield, ISO 527-2/50, Injection Molded
  • Elongation at Yield, ISO 527-2/100, Injection Molded
  • Tensile Modulus, ISO 527-2, Injection Molded
  • Flexural Strength, ISO 178, 2.0 mm/min, 3-points, Injection Molded
  • Flexural Modulus, ISO 178, 2.0 mm/min, 3-points, Injection Molded
  • Izod Impact, Notched (ISO), ISO 180/A, Injection Molded
  • Izod Impact, Notched (ISO), ISO 180/A, Injection Molded
  • Charpy Impact, Notched, ISO 179/2C, Injection Molded
  • Charpy Impact, Notched, ISO 179/1eA, Injection Molded
  • Charpy Impact, Notched, ISO 179/2C, Injection Molded
  • Charpy Impact, Notched, ISO 179/1eA, Injection Molded
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2/A, Annealed
  • Vicat Softening Point, ISO 306/B50
  • Flammability, UL94
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Trinseo, former Styron

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.