MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Evonik BREAK-THRU® Vibrant Surfactants
Categories: Fluid

Material Notes: BREAK-THRU® Vibrant is a non-ionic organic surfactant.

Application: BREAK-THRU Vibrant can be used as a tank mix adjuvant as well as an additive for in-can formulations. BREAK-THRU Vibrant imparts a very low dynamic surface tension and improves the adhesion of pesticidal sprays. In field trials, BREAK-THRU® Vibrant has proven safe for use on crops, and tests suggest good activity on pesticides used in grass crops such as cereals and rice. Manufacturer recommends a dose rate of 200-400 ml/ha. BREAK-THRU® has not proven phytotoxic in field trials, has a very low foaming potential and does not stabilize foams. Testing has also shown that the product reduces the amount of driftable spray particles when used with flat fan nozzles.

Information provided by Evonik

Vendors:
Available Properties
  • Density
  • Viscosity
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.