MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Chemical Concepts Chem-Set™ UV Stone Repair Kit Acrylic Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: ChemSet™ UV Stone Repair Kit - 10 ml Consumer Kit is used when a fast permanent repair is needed to fix scratches, chips, gouges, holes, cracks and nicks on natural and engineered stone. Fast repairs can be completed in less than three minutes. No More Discoloration/Blooming Issues. This easy-to-use UV Kit uses a UV light to cure the adhesive. Without the use of an activator spray as a curing agent you will never have issues with blooming again. Great for lighter colored stones and marbles.

The cure depends on the power of the UV lamp, its spectral output, the distance between the lamp and the components, and the transmission characteristics of the substrates. The cure quoted here was determined using a low power, hand held lamp. Most industrial UV lamps would give faster cure rate.

Information provided by Chemical Concepts™.

Vendors:
Available Properties
  • Density, uncured
  • Viscosity, uncured
  • Hardness, Shore D
  • Tensile Strength
  • Dielectric Constant
  • Dielectric Strength
  • Refractive Index, cured
  • Transmission, Visible, cured
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.