MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger SPI
Syensqo (Solvay Specialty Polymers) Ixef® 3012 Polyarylamide (PARA), Glass/carbon fibers
Categories: Polymer; Thermoplastic; Polyarylamide (PAA)

Material Notes: Glass/carbon fibers, high strength and stiffness, surface gloss

Ixef® 3012 is a carbon-fiber and glass fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than glass-fiber reinforced engineering resins. Ixef® 3012 is also electrically conductive.

Black: Ixef® 3012 BK 001

Applications: Appliance Components; Appliances; Automotive Applications; Automotive Electronics; Automotive Under the Hood; Bushings; Camera Applications; Cams; Cell Phones; Electrical/Electronic Applications; Furniture; Gears; Industrial Applications; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools

Features: Chemical Resistant; Creep Resistant; Good Dimensional Stability; High Flow; High Strength; Low Moisture Absorption; Outstanding Surface Finish; Ultra High Stiffness

Injection notes: Hot Runners: 250°C to 260°C (482°F to 500°F)
Injection Pressure: rapid
Storage
- Ixef® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Ixef® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Ixef® processing guide.
Drying
- The material as supplied is ready for molding without drying. However, If the bags have been open for longer than 24 hours, the material needs to be dried. When using a desiccant air dryer with dew point of -28°C (-18°F) or lower, these guidelines can be followed: 0.5-1.5 hour at 120°C (248°F), 1-3 hours at 100°C (212°F), or 1-7 hours at 80°C (176°F).
Injection Molding
- Ixef® compounds can be readily injection molded in most screw injection molding machines. A general purpose screw is recommended, with minimum back pressure.
- The measured melt temperature should be about 280°C (536°F), and the barrel temperatures should be around 250°C to 260°C (482°F to 500°F) in the rear zone, gradually increasing to 260°C to 280°C (500°F to 536°F) in the front zone. If hot runners are used, they should be set to 250°C to 260°C (482°F to 500°F).
- To maximize crystallinity, the temperature of the mold cavity surface must be held between 120°C and 140°C (248°F and 284°F). Molding at lower temperatures will produce articles that may warp, have poor surface appearance, and have a greater tendency to creep. Set injection pressure to give rapid injection. Adjust holding pressure and hold time to maximize part weight. Transfer from injection to hold pressure at the screw position just before the part is completely filled (95%-99%).

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density, ASTM D792, Method A
  • Water Absorption, ASTM D570
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Linear Mold Shrinkage, Transverse, ASTM D955
  • Tensile Stress, ISO 527-2
  • Elongation at Break, ISO 527-2
  • Tensile Modulus, ISO 527-2
  • Flexural Strength, ISO 178
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched (ISO), ISO 180
  • Izod Impact, Unnotched (ISO), ISO 180
  • Charpy Impact Unnotched, ISO 179, Complete Break
  • Charpy Impact Unnotched, ISO 179, Complete Break
  • Charpy Impact Unnotched, ISO 179, Complete Break
  • Charpy Impact, Notched, ISO 179, Complete Break
  • Charpy Impact, Notched, ISO 179, Complete Break
  • Charpy Impact, Notched, ISO 179, Complete Break
  • CTE, linear, Parallel to Flow, ASTM D696
  • CTE, linear, Parallel to Flow, ASTM D696
  • CTE, linear, Transverse to Flow, ASTM D696
  • CTE, linear, Transverse to Flow, ASTM D696
  • CTE, linear, Transverse to Flow, ASTM D696
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2/A, Unannealed
  • Flammability, UL94
  • Rear Barrel Temperature
  • Front Barrel Temperature
  • Melt Temperature, Injection
  • Mold Temperature
  • Drying Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.