Description: Kraton D1118 B is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 33%. It is supplied from South America in the physical form(s) identified: Kraton D1118 BT - supplied as a porous pellet dusted with talcRegion: Asia Pacific, Europe, Japan, North America, and South America Uses: Kraton D1118 B is used as a modifier of bitumen or thermoplastics and in compound formulations. It may also find use as an ingredient in formulating adhesives, sealants and coatings. Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and Roofing Information provided by Kraton® |