MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Rogers Arlon CuClad 233 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: CuClad 233 uses a medium fiberglass/PTFE ratio to balance lower dielectric constant and improved dissipation factor without sacrificing mechanical properties.
  • Cross Plied Woven Fiberglass, alternating plies are oriented 90° to each other
  • High PTFE to Glass Ratio
  • Better dielectric constant uniformity than comparable non-woven fiberglass reinforced laminates

Benefits:

  • Electrical and Mechanical isotropy in the X-Y Plane
  • Extremely Low Loss
  • Well Suited for Er Sensitive Circuits

Typical Applications:

  • Military Electronics (Radars, ECM, ESM)
  • Microwave Components (Filters, Couplers, LNAs, etc.)

Information provided by Arlon Materials for Electronics (MED); now a part of Rogers Corporation.

Vendors:
Available Properties
  • Density, ASTM D792 Method A
  • Water Absorption, IPC TM-650 2.6.2.2
  • Outgassing - Total Mass Loss, NASA SP-R-0022A, Water Vapor Recovered
  • Outgassing - Total Mass Loss, NASA SP-R-0022A
  • Collected Volatile Condensable Material, NASA SP-R-0022A
  • Tensile Strength, ASTM D882, Cross
  • Tensile Strength, ASTM D882, Machine
  • Modulus of Elasticity, ASTM D638, Cross
  • Modulus of Elasticity, ASTM D638, Machine
  • Flexural Modulus, ASTM D790
  • Compressive Modulus, ASTM D695
  • Peel Strength, IPC TM-650 2.4.8, After Thermal Stress
  • Volume Resistivity, IPC TM-650 2.5.17.1, C96/35/90
  • Surface Resistance, IPC TM-650 2.5.17.1, C96/35/90
  • Dielectric Constant, IPC TM-650 2.5.5.3, C23/50
  • Dielectric Constant, IPC TM-650 2.5.5.5, C23/50
  • Dielectric Breakdown, ASTM D149, D48/50
  • Dissipation Factor, IPC TM-650 2.5.5.5, C23/50
  • Arc Resistance, ASTM D495, D48/50
  • CTE, linear, IPC TM-650 2.4.24, x direction
  • CTE, linear, IPC TM-650 2.4.24, y direction
  • CTE, linear, Transverse to Flow, IPC TM-650 2.4.24, z direction
  • Thermal Conductivity, ASTM E1225
  • Flammability, UL94, Vertical Burn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.