MARPOL® LDM 733 is a high flow, low density PE homopolymer resin designed to provide good processability. It is suitable for use in making color concentrates and injection molded items. Recommended Applications: caps, closures, compounding, food packaging containers, houseware articles, injection molding and masterbatch base resin. Additives: Slip- no, Antiblock – no. Information provided by Marco Polo International, LLC |