MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Wefapress St 6000® ELS FDA Electroconductive PE-UHMW
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: St 6000® ELS FDA FSP is an ultra-high molecular weight low pressure polyethylene (PE-UHMW) with a molecular weight of approximately 9.2 million g/mol. St 6000® ELS FDA FSP (electrically conductive, stabilized) has a surface resistance of < 103, which is achieved by means of a high proportion of lampblack. This fills the gap between antistatic (AST) and ATEX (Atmosphere Explosive) applications. Properties: Electro conductive, FDA-approved, Good sliding properties, High wear resistance, Zero moisture absorption, Conforms to EU 10/2011 (FSP variant), Excellent impact resistance.

Applications: Components for the food industry, Star configuration conveyors, Guide rails, Sliding profiles, slide bearings, slide rails, Shock and impact resistant parts. Industries: Conveyor systems and automation, Drinks and bottling industries, Mechanical and plant engineering, Food industry.

Information provided by Wefapress.

Vendors:
Available Properties
  • Density, DIN 53479
  • Moisture Absorption
  • Molecular Weight
  • Hardness, Shore D, DIN 53505
  • Ball Indentation Hardness, DIN ISO 2039 Teil 1
  • Tensile Strength, DIN 53455
  • Tensile Strength, Ultimate, DIN 53455
  • Elongation at Break, DIN ISO / R 527
  • Modulus of Elasticity, DIN 53457
  • 1% Secant Modulus, EU 1935/2004 - EU 10/2011 (FSP Quality)
  • Charpy Impact, Notched, DIN 53457
  • Coefficient of Friction
  • Sand Slurry, % Abrasion
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • CTE, linear, DIN ISO 11359
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point, DTA
  • Maximum Service Temperature, Air, DIN 53461, Dimensional Stability
  • Maximum Service Temperature, Air, Continuous Application Temp.
  • Vicat Softening Point, DIN 53460
  • Minimum Service Temperature, Air
  • Flammability, UL94
  • FDA
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.