MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Eastman 1925F Polyethylene Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Polyethylene 1925F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good clarity is important. Common applications include bread bags, fresh produce bags, and converter film requiring printability. An additive in this formulation limits the use of 1925F to nonalcoholic foods, and the average thickness of such polymers in the form in which they contact food shall not exceed 0.0050 inch. Users must make their own determination of its safety, lawfulness, and technical suitability in their intended applications.

Applications/Uses

  • Bread bags
  • Produce bags
  • Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.

    Vendors:
    Available Properties
    • Base Resin Density, ASTM D4883
    • Water Vapor Transmission, ASTM F372
    • Oxygen Transmission, ASTM D3985
    • Thickness
    • Base Resin Melt Index, ASTM D1238
    • Film Tensile Strength at Yield, MD, ASTM D882
    • Film Tensile Strength at Yield, TD, ASTM D882
    • Film Elongation at Break, MD, ASTM D882
    • Film Elongation at Break, TD, ASTM D882
    • Coefficient of Friction, ASTM D1894
    • Elmendorf Tear Strength, MD, ASTM D1922
    • Elmendorf Tear Strength, TD, ASTM D1922
    • Dart Drop, ASTM D1709
    • Film Tensile Strength at Break, MD, ASTM D882
    • Film Tensile Strength at Break, TD, ASTM D882
    • 1% Secant Modulus, MD, ASTM D882
    • 1% Secant Modulus, TD, ASTM D882
    • Vicat Softening Point, ASTM D1525
    • Haze, ASTM D1003
    • Gloss, ASTM D2457, at 45°
    • Transmission, Visible, ASTM D1746, Transparency
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    Eastman Chemical Company

    Category Notes
    Plastic

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Rulon Bearings
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.