MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Trinseo PULSE™ GX50 PC/ABS Engineering Resin
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: PULSE™ GX50 is an easy flow, medium-heat, low density PC/ABS resin delivering optimized performance for automotive interior component applications.

Benefits:

  • Low gloss allowing paint-less visible applications
  • Low density driving to lighter and cost optimized parts
  • Easy flow, reduced scrap, and faster cycle times, while enabling thing wall part design for mass reduction
  • High-impact strength even at low temperature
  • Heat resistance optimized for the majority of automotive interior components
  • Consistent natural white color produces high quality part appearance when used with color concentrates (self coloring) or Trinseo Color Masterbatch Technology
  • Low odor & VOC to meet all global Automotive OEM specifications
Applications:
  • Mid (floor) consoles
  • Lower Instrument Panel components
  • Door panel trim
  • Pillars
  • Storage/load floors/glove box
Automotive Specifications:
  • BMW GS 93016
  • DAIMLER DBL 5404.83
  • GM GMW15581P-ABS+PC-T1
  • GM GMW15581P-ABS+PC-T4
  • HONDA HSM-C4-G (EU)
  • PSA Peugeot-Citroen FTM 62 0008
  • TESLA TM-1003 10/20
  • VOLKSWAGEN TL 522 31
  • VOLVO STD 1212,86

Information provided by Trinseo.

Vendors:
Available Properties
  • Density, ISO 1183/B
  • Volatile Organic Compounds (VOC) Content, VDA 277, 10 µg/g
  • Apparent Bulk Density, ISO 60
  • Linear Mold Shrinkage
  • Melt Flow, ISO 1133
  • Spiral Flow, Injection Pressure: 1.8E+3 bar
  • Tensile Strength, Yield, ISO 527-2/50
  • Elongation at Break, ISO 527-2/50
  • Tensile Modulus, ISO 527-2, 1 mm/min
  • Charpy Impact, Notched, ISO 179/1eA
  • Charpy Impact, Notched, ISO 179/1eA
  • CTE, linear, Parallel to Flow, ISO 11359-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2/A, Unannealed
  • Vicat Softening Point, ISO 306/B50
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Trinseo, former Styron

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.