DuPont™ Elvaloy® 741WR an ethylene/vinyl acetate/carbon monoxide (E/VA/CO) copolymer. The difference between Elvaloy®741 and Elvaloy®741WR, is that Elvaloy®741WR contains a wax additive to deter pellet blocking in packaging/distribution/handling. DuPont™ ELVALOY® 741WR Resin Modifier complies with Food and Drug Administration Regulation 21 CFR 175.105 - - Adhesives. This Regulation describes adhesives that may be used as components of articles intended for use in packaging, transporting, or holding food, subject to the limitations and requirements therein. This former DuPont product line is now a Dow product line. |