MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Fibre Glast 83 Waxed Polyester Laminating Resin
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: Description: #83 Waxed Polyester Laminating Resin is a prepromoted, thixotropic general purpose resin. #83 contains styrene wax for low styrene emissions and to prevent air inhibition. #83 is a waxed resin for laminating thin fiberglass skins on plywood, or for general purpose fiberglass repairs. The wax in the resin will prevent surface tackiness even when applied in thin coats. Sand off the wax layer before painting or secondary bonding.

Performance:
  • High thixotropic index to prevent draining in vertical surfaces
  • Low viscosity for fast wet out
  • Styrene suppressed

Suggested Uses:#83 Polyester Molding Resin can be used for hand lay-up or spray-up for general fiberglass reinforced plastics applications.

Information provided by Fibre Glast Developments Corporation.

Vendors:
Available Properties
  • Solids Content
  • Brookfield Viscosity, #2 Spindle, 30 rpm
  • Flash Point
  • Cure Time, using 1.25% #69 Catalyst
  • Gel Time, At 77°F using 1.25% #69 Catalyst
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Fibre Glast Developments Corporation

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.