MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Vesta Ceramics SicoMill® Grade 4 Silicon Powder  (discontinued **)
Categories: Metal; Nonferrous Metal; Other Engineering Material; Semiconductor

Material Notes: General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single customer’s specifications and use. We have developed and improved the production line for the SicoMill® enabling us to follow the manufacture of our products at all stages with even greater certainty ensuring that the final product is consistent at all times.

Vendors:
Available Properties
  • Bulk Density, Size E (apparent)
  • Bulk Density, Size D (apparent)
  • Bulk Density, Size C (apparent)
  • Bulk Density, Size E (tapped)
  • Bulk Density, Size D (tapped)
  • Bulk Density, Size B (apparent)
  • Bulk Density, Size C (tapped)
  • Bulk Density, Size B (tapped)
  • Particle Size, D10 (Malvern) Size E
  • Particle Size, D10 (Malvern) Size D
  • Particle Size, D10 (Malvern) Size C
  • Particle Size, D50 (Malvern) Size E
  • Particle Size, D50 (Malvern) Size D
  • Particle Size, D90 (Malvern) Size E
  • Particle Size, D10 (Malvern) Size B
  • Particle Size, D50 (Malvern) Size C
  • Particle Size, D90 (Malvern) Size D
  • Particle Size, 99.9% less than value (Size E)
  • Particle Size, D90 (Malvern) Size C
  • Particle Size, 98% less than value (Size C)
  • Particle Size, 99.5% less than value (Size D)
  • Particle Size, D50 (Malvern) Size B
  • Particle Size, D90 (Malvern) Size B
  • Particle Size, 98% less than value (Size B)
  • Specific Surface Area, Size B
  • Specific Surface Area, Size C
  • Specific Surface Area, Size D
  • Specific Surface Area, Size E
  • Aluminum, Al
  • Calcium, Ca
  • Carbon, C
  • Iron, Fe
  • Oxygen, O
  • Silicon, Si
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.