MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Total XLS 12 B High Density Polyethylene - Pipes and Fittings
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: HDPE XLS 12 B is a high performance hexene-based black compound, with a MRS 10 MPa - PE100 classification, primarily intended for extrusion of large diameter and thick wall pressure pipes.

Key characteristics are

  • a superior resistance to sagging, enabling the manufacture of very thick wall pipes with even wall distribution
  • an outstanding resistance to slow crack growth an rapid crack propagation ensuring safe and long-term network operation
  • an optimized formulation of additives and finely dispersed carbon black providing outstanding long-term stability in service

Designation ISO 1872-PE,E/M-ACGHL,50-T003

Information provided by Total Petrochemicals.

Vendors:
Available Properties
  • Specific Gravity, ISO 1183
  • Carbon Black Loading, ISO 6964
  • Melt Flow, ISO 1133/T
  • Melt Temperature, Extrusion
  • Melt Temperature, Injection
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Total Atofina

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.