Description: Thermoplastic elastomer SEBS block copolymer 511 has low melt viscosity, excellent resilience, good compatibility with a variety of inorganic fillers and organic polar materials. SEBS polymer 511 can be used for wires, seals, and soft materials in contact with foods. Application: Plastic modification/Compounding/Cable/Wire/Sealants/Food Formula: Molars SEBS polymer 511: 30 paraffinic oil (food grade): 45 PP (health grade): 25 Antioxidant: 0.2% Information provided by BEC Materials, LLC |