MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Chesterton ARC 982 100% Novolac acid resistant coating  (discontinued **)
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. A low viscosity composite that is applied by brush, squeegee, or a plural component sprayer system. ARC 982 may be applied at a minimum thickness of 250 microns (10 mils) per coat. A two-coat application of ARC 982 provides protection from concentrated acids, alkailes, and solvents. The cured composite provides outstanding chemical resistance with a high gloss finish.

Benefits:

  • Excellent resistance to a wide variety of concentrated acids such as sulfuric acid up to 98% and fluctuating chemical environments.
  • ARC 982 outlasts rubber and other traditional lining materials as it is resistant to aging and embrittlement
  • Tough resin structure resists thermal-mechanical shock
  • Outstanding adhesion results in reliable performance with no under film corrosion
  • Holiday testable per NACE RP0188

Suggested Uses:

  • Chemical Storage Tanks
  • Exhaust Gas Ductwork
  • Impellers
  • Pump Casings
  • Structural Steel
  • Valves
  • Chimneys and Stacks
  • Fans and Housings
  • Heat Exchangers
  • Tanks and Piping
  • Reaction Vessels

Information provided by Chesterton

Vendors:
Available Properties
  • Density, Cured
  • Hardness, Shore D, ASTM D2240
  • Elongation at Break, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695
  • Adhesive Bond Strength, ASTM D4541
  • Impact Test, ASTM D2794, Reverse
  • Impact Test, ASTM D2794, Direct
  • CTE, linear, ASTM C531
  • Maximum Service Temperature, Air, Wet Service
  • Maximum Service Temperature, Air, Dry Service
  • Cure Time, Light Load/Overcoat End
  • Cure Time, Light Load/Overcoat End
  • Cure Time, Light Load/Overcoat End
  • Cure Time, Full Load
  • Cure Time, Full Load
  • Cure Time, Light Load/Overcoat End
  • Cure Time, Full Load
  • Cure Time, Full Load
  • Cure Time, Chemical Resistance
  • Cure Time, Chemical Resistance
  • Cure Time, Chemical Resistance
  • Cure Time, Chemical Resistance
  • Tack-Free Time
  • Tack-Free Time
  • Tack-Free Time
  • Tack-Free Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.