Additive: Plasticizer
Features: Good Flexibility; High Impact Resistance; Hydrolysis Resistant; Plasticized; UV Resistant
Uses: Automotive Applications; Consumer Applications; Hydraulic Applications; Industrial Applications; Pneumatic Applications
RoSH Compliance: RoSH Compliant
Automotive Specifications: PSA Peugeot-Citroen SPA X62 4127 Color: 9992 Black
Forms: Granules
Processing Method: Extrusion
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticPA, Polyamide