MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Go Yen Chemical GY-NA-2000 Nucleating Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro:
  • GY-NA-2000 series are new class of nucleating agents capable of inducing crystal growth in the polymer. This series product act as a nucleating agent by creating a large number of small size crystalline structure during the cooling of the polypropylene melt
  • GY-NA-2000 series improves mechanical properties, clarity of polypropylene, heat resistance, size stability and surface gloss.
  • GY-NA-2000 series product make injection molders achieve better production speeds and broaden the molding condition.
Features:
  • Enhance the mechanical strength
  • Improve crystal growth in the polymer
  • Improve the clarity of goods
  • Provide long-term heat stability
  • Enhance the stability of melting for polymers.
  • By using GY-NA-2000 series, it can be anti-aging, antifragile during the processing of organic polymer.
Applications:
  • PP (Polypropylene)
  • PET (Polyethylene terephthalate)
  • PBT (Polybutylene terephthalate)
  • PC (Polycarbonate)
  • PMMA (Polymethyl Methacrylate)
  • Polyamide
  • Polyolefin( HDPE , LDPE , EVA , PVC )
  • Others & Elastomer (TPU,TPE.TPV.SBS)
GY-NA-2000 series can be blended with Polypropylene directly or add it in the pellet manufacturing.

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • Tensile Strength
  • Impact, [kg/m2], Impact resistance ratio
  • Haze
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.