MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Syensqo (Solvay Specialty Polymers) Hyflon® MFA D5220X Perfluoropolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; TFE/Perfluoromethylvinylether Copolymer (MFA)

Material Notes: Hyflon D5220X is a white aqueous MFA dispersion. It is designed for impregnation processes and is particularly recommended for production of fabrics and laminates. Hyflon D5220X exhibits excellent wetting properties and high shear stability. Hyflon D5220X has very good film forming behaviour and is especially suited for top-coat passes to produce final items with superior gloss. Due to its features, D5220X can of course also find use in formulations for coating applications. Main features of Hyflon D5220X MFA dispersion are: - Very low APFO content - NO polyethoxylated alkylphenols - Excellent wetting properties - Superior gloss of final items

Additional Information: Processing - Hyflon D5220X is processed according to methods generally used for conventional impregnation technology. Generally the procedure involves dip-coating and then heating to remove water and surfactant from the impregnated item. Depending on the application, sintering above the melting point of the coated resin may be carried out to obtain the finished coated articles. - Hyflon D5220X can be processed neat or appropriately formulated. Also, it can be used diluted using distilled or deionized water. Formulation, line speed and oven temperature must all be well controlled for optimized features of the coated substrates. Storage and Handling - Hyflon MFA dispersions must be stored under suitable temperature conditions to ensure prolonged stability. Temperatures lower than 5°C must be avoided to prevent irreversible settling. Also, some settling may occur on prolonged standing and/or heat exposure. It is therefore strongly recommended that the product is always kept at temperatures below 35°C. The optimum storage temperature range is 10 - 25°C. It is also advisable that the product is homogenized by gentle rolling or stirring once per month and prior to use. - Prolonged exposure of the liquid to air could lead to some coagulation at the surface due to water evaporation. For this reason and also to avoid contamination, it is recommended to keep the containers closed when not in use. Safety and Toxicology - Before using Hyflon MFA dispersions consult the product Material Safety Data Sheet and follow all label directions and handling precautions. - As with all PTFE materials, handling and processing should only be carried out in well ventilated areas. Venting units should be installed above processing equipment. Fumes must not be inhaled and eye and skin contact ought to be avoided. In case of skin contact wash with soap and water. In case of eye contact flush with water immediately and seek medical help. Do not smoke in areas contaminated with powder, vapour or fumes. See Material Safety Data Sheet for detailed advice on waste disposal methods. Packaging - Hyflon D5220X is packaged in either 25 kg drums or 1500 kg IBC's.

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density, ASTM D4441
  • Particle Size, Internal Method, Average
  • pH, ASTM D4441
  • Brookfield Viscosity, ASTM D2196, 20°C
  • Melting Point, ASTM D4591
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.