Features: General Purpose; Good Colorability; Good Flexibility; Halogen Free, High Elasticity; High Elongation; High Tensile Strength; Low Flow; Low Temperature Flexibility; Low Temperature Toughness; Ozone Resistant; Sunlight Resistant (720 hours); UV Resistant; Weather Resistant
Notes: RoHS Compliant
Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Electrical/Electronic Applications; Industrial Cable Jacketing; Terminal Cable Jacketing; Underground Power Cable; Wire and Cable Applications; Wire Jacketing
Wire Types: SJEOW
Agency Ratings: UL 1581; QMTT2.E73402
Forms: Pellets
Processing Method: Extrusion; Injection Molding
Injection Notes: Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C); Injection Rate: Moderate-Fast
Extrusion Notes: Screw Speed: 30 to 100 rpm
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticThermoplastic Elastomer